e than 265 ℃, peak welding time dont more than 3 seconds, and at the same time, reflow welding machine Taiwan to esd and electrostatic eliminating.
8 in the welding temperature returned to normal before, must avoid make LED by any vibration or external forces.
And this product is suitable for reflow soldering.
10 is the single guide LED many before installation confirm if the polarity, installed in voltage was easy to cause injury or failure LED chips.
11 circuit design, please avoid LED and he